Sintering of ZYP powder particles starts around 900°C and it is possible to create zirconia ceramic parts approaching theoretical density using ZYP at only 1450°C.

This ultra-fine powder is particularly appreciated in filtration, the manufacture of oxygen sensors, thermal barrier coatings for gas turbines and diesel engines, polishing and as grain growth inhibitor for non-oxide ceramics.

  • ZrO2 : 90%

  • Y2O3 : 10%

  • Impurities : < 1%

  • Ignition loss : 1,8%

  • Specific surface area : 25-35 m²/g